The surface of solid ceramic brick was hydrophobized with apreparation based on nanopolymers with added nanosilica. The effect of hydrophobization on the surface durability was evaluated. The surface hardness was determined after seasoning of the samples for 14 days and 20 cycles of immersion in water followed by drying.
Fic, S., Kłonica, M., & Szewczak, A. (2021). Effect of hydrophobization on the durability of building ceramics. Polimery, 61(1), 46–48. https://doi.org/10.14314/polimery.2016.046